NMC532 Double-Sided Cathode Electrode Sheet
Specification: 241 mm L × 200 mm W
Application: Lithium-ion Battery Electrode Material
|
Item No. |
Package |
|
01013503 |
5 sheets/package |
Description: NMC532 Series Double-Sided Cathode Electrode Sheet
Main Specifications
|
Item |
Specification |
|
Electrode Sheet Dimensions |
241 mm (L) × 200 mm (W) |
|
Coated Area |
241 mm (L) × 175 mm (W) (12.5 mm uncoated margin on each side) |
|
Coating Type |
Double-sided coating |
|
Current Collector Thickness |
16 μm |
|
Coating Areal Density |
23 ± 0.4 mg/cm² |
|
Aluminum Foil Areal Density |
4.22 mg/cm² |
|
Calendered Density |
3.4 ± 0.1 g/cm³ |
|
Active Material Content |
95.5 wt.% |
|
Typical Specific Capacity |
160 mAh/g |
|
Recommended Voltage Range |
3.0–4.3 V |
|
Active Material Mass Calculation |
Coating areal density × active material content × electrode sheet area |
|
Storage Instructions |
After opening the package, reseal it immediately. The electrode sheets may be dried at 60°C or stored in a glove box. |
Packaging and transportation
Packaging material: cardboard box.
Packaging method: Vacuum sealed packaging.
Pay attention to moisture-proof, waterproof, and light proof storage.
Transportation requirements: prevent collision, compression, moisture, sun protection, and damage.
Storage environment(electrode packaging in sealed state)
Temperature: -40 ℃~60 ℃
Relative humidity: 75% RH Max
The shelf life: 12 months.